Applicable to carbon, sulfur, chromium, molybdenum, nickel, silicon, iron, magnesium, copper, zinc, manganese, phosphorus, tin, aluminum, rare earths, titanium, cobalt, calcium in all types of metal (high manganese steel, carbon steel, raw cast iron, stainless steel, alloy steel, etc.) materials, and other elements of laboratory analysis .
I.Main technical parameters
1. Analytical range
C: 0.001-10.0000% S: 0.0005-5.0000% Cr: 0.01%-70%
Ni: 0.01%-90% Mo: 0.01%-75% Si: 0.001%-60%
Fe: 0.01%-90% Mn: 0.001%-90% Cu: 0.01%-90%
Al: 0.01%-80% Ti: 0.01%-45% P: 0.001%-20%
Co: 0.01%-80% Mg: 0.01%-30% Ca: 0.01%-40%
2. Analysis time: 45s
3. Analysis error: C is better than GB/T223.69-2008 standard, S is better than GB/T223.68-1997 standard, accord with GB223.3-5-88 standard.
4. Power supply: 220V±10% 50Hz
5. Power consumption: around 50VA
6. Power gas: oxygen, pressure 20~40KPa
7. Ambient temperature: -5℃~40℃
8. Net weight: around 80kg